Hydroxyethyl Cellulose (HEC)mai kauri ne, stabilizer da rheology regulator wanda aka saba amfani dashi a fenti na latex. Yana da wani ruwa mai narkewa polymer fili samu ta hanyar hydroxyethylation dauki na halitta cellulose, tare da mai kyau ruwa solubility, rashin guba da muhalli kariya. A matsayin muhimmin sashi na fenti na latex, hanyar ƙari na hydroxyethyl cellulose kai tsaye yana shafar kaddarorin rheological, aikin gogewa, kwanciyar hankali, mai sheki, lokacin bushewa da sauran mahimman kaddarorin fenti na latex.

 1

1. Tsarin aikin hydroxyethyl cellulose

Babban ayyukan hydroxyethyl cellulose a cikin tsarin fenti na latex sun haɗa da:

Ƙarfafawa da kwanciyar hankali: Ƙungiyoyin hydroxyethyl a kan sarkar kwayoyin halitta na HEC suna samar da haɗin gwiwar hydrogen tare da kwayoyin ruwa, wanda ke haɓaka hydration na tsarin kuma ya sa fenti na latex ya sami mafi kyawun halayen rheological. Hakanan yana haɓaka kwanciyar hankali na fenti na latex kuma yana hana ɓarna na pigments da filler ta hanyar yin hulɗa tare da sauran kayan abinci.

Tsarin Rheological: HEC na iya daidaita kaddarorin rheological na fenti na latex kuma inganta haɓakar dakatarwa da kaddarorin fenti. A ƙarƙashin yanayi daban-daban, HEC na iya nuna nau'in ruwa daban-daban, musamman ma a ƙananan ƙananan ƙira, zai iya ƙara danko na fenti, hana hazo, da tabbatar da daidaito na fenti.

Rashin ruwa da riƙewar ruwa: Rashin ruwa na HEC a cikin launi na latex ba zai iya ƙara yawan danko ba, amma kuma ya tsawaita lokacin bushewa na fim din fenti, rage raguwa, da kuma tabbatar da kyakkyawan aikin fenti a lokacin ginawa.

 

2. Ƙara hanyar hydroxyethyl cellulose

Hanyar ƙari naHECyana da tasiri mai mahimmanci akan aikin ƙarshe na fenti na latex. Hanyoyin ƙari na gama gari sun haɗa da hanyar ƙara kai tsaye, hanyar rushewa da hanyar watsawa, kuma kowace hanya tana da fa'idodi da rashin amfani daban-daban.

 

2.1 Hanyar ƙara kai tsaye

Hanyar ƙari kai tsaye ita ce ƙara hydroxyethyl cellulose kai tsaye zuwa tsarin fenti na latex, kuma yawanci yana buƙatar isasshen motsawa yayin tsarin hadawa. Wannan hanya mai sauƙi ne kuma mai sauƙi don aiki, kuma ya dace da samar da fenti na latex. Duk da haka, lokacin da aka kara kai tsaye, saboda manyan ƙwayoyin HEC, yana da wuya a narke da tarwatsawa da sauri, wanda zai iya haifar da haɓakar ƙwayar cuta, yana shafar daidaituwa da halayen rheological na fenti na latex. Don kauce wa wannan halin da ake ciki, ya zama dole don tabbatar da isasshen lokacin motsawa da kuma zafin jiki mai dacewa a lokacin tsarin ƙari don inganta rushewa da watsawa na HEC.

 

2.2 Hanyar warwarewa

Hanyar narkar da ita ita ce narkar da HEC a cikin ruwa don samar da bayani mai mahimmanci, sa'an nan kuma ƙara maganin zuwa fenti na latex. Hanyar narkar da ita na iya tabbatar da cewa HEC ta narkar da shi, guje wa matsalar haɓakar barbashi, da kuma ba da damar HEC ta rarraba a ko'ina a cikin fenti na latex, yana wasa mafi kyawun kauri da daidaitawar rheological. Wannan hanyar ta dace da samfuran fenti na ƙarshen ƙarshen latex waɗanda ke buƙatar kwanciyar hankali mafi girma da kaddarorin rheological. Koyaya, tsarin rushewar yana ɗaukar lokaci mai tsawo kuma yana da manyan buƙatu don saurin motsawa da zafin jiki na narkewa.

 

2.3 Hanyar watsawa

Hanyar watsawa ta haɗu da HEC tare da wasu additives ko kaushi da kuma tarwatsa shi ta amfani da manyan kayan watsawa mai ƙarfi don yin HEC a ko'ina a rarraba a cikin fenti na latex. Hanyar watsawa na iya yadda ya kamata ya guje wa agglomeration na HEC, kula da kwanciyar hankali na tsarin kwayoyin halitta, da kuma kara inganta kaddarorin rheological da aikin gogewar fenti na latex. Hanyar watsawa ta dace da samar da manyan ayyuka, amma yana buƙatar yin amfani da kayan aikin ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararrun ƙwararru , kuma kula da yanayin zafi da lokaci a lokacin aikin watsawa yana da matukar damuwa.

 2

3. Tasirin Hanyar Ƙara Hydroxyethyl Cellulose akan Ayyukan Fenti na Latex

Hannun ƙari na HEC daban-daban za su shafi manyan kaddarorin fenti na latex masu zuwa:

 

3.1 Rheological Properties

A rheological Properties naHECmabuɗin aiki ne na fenti na latex. Ta hanyar nazarin hanyoyin ƙarin HEC, an gano cewa hanyar rushewa da hanyar watsawa na iya inganta halayen rheological na fenti na latex fiye da hanyar ƙari kai tsaye. A cikin gwajin rheological, hanyar rushewa da hanyar watsawa za su iya inganta danko na fenti na latex a ƙananan ƙarancin ƙarfi, don haka fentin latex yana da kyau mai kyau da kuma abubuwan dakatarwa, kuma ya guje wa sabon abu na sagging yayin aikin ginin.

 

3.2 Kwanciyar hankali

Hanyar ƙari na HEC yana da tasiri mai mahimmanci akan kwanciyar hankali na fenti na latex. Fenti na latex ta amfani da hanyar narkar da hanyar watsawa yawanci sun fi karko kuma suna iya hana lalatawar pigments da filler yadda ya kamata. Hanyar ƙari na kai tsaye yana da sauƙi ga rarrabawar HEC maras kyau, wanda hakan yana rinjayar kwanciyar hankali na fenti, kuma yana da haɗari ga lalatawa da ƙaddamarwa, rage rayuwar sabis na fenti na latex.

 

3.3 Abubuwan rufewa

Abubuwan da aka rufe sun haɗa da daidaitawa, ƙarfin rufewa da kauri daga cikin sutura. Bayan hanyar rushewa da hanyar watsawa an karɓa, rarraba HEC ya fi dacewa, wanda zai iya sarrafa daidaitaccen ruwa na rufin kuma ya sa suturar ta nuna kyakkyawan matakin daidaitawa da mannewa yayin aikin sutura. Hanyar ƙari kai tsaye na iya haifar da rarrabawar ƙwayoyin HEC marasa daidaituwa, wanda hakan yana rinjayar aikin shafi.

 

3.4 Lokacin bushewa

Riƙewar ruwa na HEC yana da tasiri mai mahimmanci akan lokacin bushewa na fenti na latex. Hanyar rushewa da hanyar watsawa na iya zama mafi kyawun kiyaye danshi a cikin fenti na latex, tsawaita lokacin bushewa, da kuma taimakawa wajen rage yawan bushewa da fashewa yayin aikin sutura. Hanyar ƙari kai tsaye na iya haifar da wasu HEC da ba su cika narkar da su ba, ta yadda za su shafi daidaitaccen bushewa da ingancin fenti na latex.

 3

4. Shawarwari ingantawa

Hanyoyi daban-daban na ƙarawahydroxyethyl cellulosesuna da tasiri mai mahimmanci akan aikin tsarin fenti na latex. Hanyar rushewa da hanyar watsawa suna da sakamako mafi kyau fiye da hanyar ƙari kai tsaye, musamman a inganta kayan aikin rheological, kwanciyar hankali da aikin sutura. Don haɓaka aikin fenti na latex, ana ba da shawarar yin amfani da hanyar rushewa ko hanyar watsawa yayin aikin samarwa don tabbatar da cikakken rushewa da rarrabuwa iri-iri na HEC, don haka inganta ingantaccen aikin fenti na latex.

 

A cikin ainihin samarwa, ya kamata a zaɓi hanyar ƙari na HEC mai dacewa bisa ga takamaiman tsari da manufar fenti na latex, kuma a kan wannan, aiwatar da motsawa, narkewa da tarwatsawa ya kamata a inganta su don cimma kyakkyawan aikin fenti na latex.